Grade X20CrMoWV 12-1
European Standard Steel Grade 1.4935
Corresponding Standard EN 10302-2008
Creep resisting steels,nickel and cobalt alloys
Classification Martensitic Stainless Steel
Properties Corrosion Resistance
X20CrMoWV 12-1 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Mo W V
Minimum Value 0.17 0.1 0.3 - - 11 0.3 0.8 0.4 0.2
Maximum Value 0.24 0.5 0.8 0.025 0.015 12.5 0.8 1.2 0.6 0.35
X20CrMoWV 12-1 Mechanical Properties
width
b
mm
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
-* +QT 700 700~850 ≥500 ≥16
b≥3** +QT 700 700~850 ≥500 ≥15
-* +QT 800 800~950 ≥600 ≥14
Approximate Comparison Table Martensitic Heat-Resistant Steel
China Taiwan, China Japan South Korea United States Germany
GB ISC CNS JIS KS ASTM UNS DIN EN/DIN W-Nr.
22Cr12NiWMoV
(2Cr12NiWMoV)
S47220 SUH 616 SUH 616 STR 616 616 S42200 X20CrMoWV 12-1 1.4935
X20CrMoWV12-1 Corresponding Standards(Same grade name, different standards)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!