USA UNS N08367
Corresponding Standard ASTM A479/A479M-2018
Standard Specification for Stainless Steel Bars and Shapes for Use in Boilers and Other Pressure Vessels
Classification Austenitic Stainless Steel
Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu Mo N
Minimum Value - - - - - 20 23.5 - 6 0.18
Maximum Value 0.03 1 2 0.04 0.03 22 25.5 0.75 7 0.25
◎ New designations established in accordance with Practice E527 and SAE J1086 published jointly by ASTM and SAE. See ASTM DS-56C, available from ASTM Headquarters.
Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
All specifications Annealing ≥655 ≥310 in 2 in.[50 mm] or 4D
≥ 30
≤241
◎ d-diameter, t-thickness
Approximate Comparison Table Austenitic Stainless Steel
Japan United States International Organization for Standardization European Standard
JIS UNS ISO Numerical Grade Numerical Grade
SUS836L N08367 X2NiCrMoN25-21-7 4478-083-67-U (1.4478)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!