USA UNS S24000
ASTM
Specification or Grade
XM-29
Corresponding Standard ASTM A479/A479M-2018
Standard Specification for Stainless Steel Bars and Shapes for Use in Boilers and Other Pressure Vessels
Classification Austenitic Stainless Steel
Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni N
Minimum Value - - 11.5 - - 17 2.3 0.2
Maximum Value 0.08 1 14.5 0.06 0.03 19 3.7 0.4
◎ New designations established in accordance with Practice E527 and SAE J1086 published jointly by ASTM and SAE. See ASTM DS-56C, available from ASTM Headquarters.
Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Reduction of Area
ψ
%
All specifications Annealing ≥690 ≥380 in 2 in.[50 mm] or 4D
≥ 30
≥ 50 ①
◎ d-diameter, t-thickness

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!