USA UNS S30409
ASTM
Specification or Grade
304H
Corresponding Standard ASTM A479/A479M-2018
Standard Specification for Stainless Steel Bars and Shapes for Use in Boilers and Other Pressure Vessels
Classification Austenitic Stainless Steel
Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni
Minimum Value 0.04 - - - - 18 8
Maximum Value 0.1 1 2 0.045 0.03 20 10.5
◎ New designations established in accordance with Practice E527 and SAE J1086 published jointly by ASTM and SAE. See ASTM DS-56C, available from ASTM Headquarters.
Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Reduction of Area
ψ
%
All specifications Annealing ≥ 515 ① ≥205 in 2 in.[50 mm] or 4D
≥ 30
≥ 40 ②
◎ d-diameter, t-thickness
1 Approximate Comparison Table Austenitic Stainless Steel
China Japan United States International Organization for Standardization Germany European Standard
GB ISC JIS AISI UNS ISO DIN EN/DIN W-Nr. EN Numerical Grade
07Cr19Ni10 S30409 SUS 304H 304H S30409 X6CrNi 18-10
X7CrNi 18-9
X6CrNi18-10 1.4948 X6CrNi18-10 1.4948
2 Approximate Comparison Table
Japan United States International Organization for Standardization France European Standard Russia
JIS ASTM UNS ISO NF EN/NF EN Numerical Grade GOST
SUS304H 304H S30409 X7CrNi18-9 Z6CN18-09 X6CrNi18-10 1.4948 08KH18N10