USA UNS S30909
ASTM
Specification or Grade
309H
Corresponding Standard ASTM A479/A479M-2018
Standard Specification for Stainless Steel Bars and Shapes for Use in Boilers and Other Pressure Vessels
Classification Austenitic Stainless Steel
Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni
Minimum Value 0.04 - - - - 22 12
Maximum Value 0.1 1 2 0.045 0.03 24 15
◎ New designations established in accordance with Practice E527 and SAE J1086 published jointly by ASTM and SAE. See ASTM DS-56C, available from ASTM Headquarters.
Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Reduction of Area
ψ
%
All specifications Annealing ≥ 515 ① ≥205 in 2 in.[50 mm] or 4D
≥ 30
≥ 40 ②
◎ d-diameter, t-thickness

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!