USA UNS S31266
Corresponding Standard ASTM A479/A479M-2018
Standard Specification for Stainless Steel Bars and Shapes for Use in Boilers and Other Pressure Vessels
Classification Austenitic Stainless Steel
Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu Mo N W
Minimum Value - - 2 - - 23 21 1 5.2 0.35 1.5
Maximum Value 0.03 1 4 0.035 0.02 25 24 2.5 6.2 0.6 2.5
◎ New designations established in accordance with Practice E527 and SAE J1086 published jointly by ASTM and SAE. See ASTM DS-56C, available from ASTM Headquarters.
Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
All specifications Annealing ≥750 ≥420 in 2 in.[50 mm] or 4D
≥ 35
◎ d-diameter, t-thickness
Approximate Comparison Table Austenitic Stainless Steel
United States International Organization for Standardization European Standard
UNS ISO Numerical Grade Numerical Grade
S31266 X1CrNiMoCuNW24-22-6 4659-312-66-I 1.4659

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!