USA UNS S31651
ASTM
Specification or Grade
316N
Corresponding Standard ASTM A479/A479M-2018
Standard Specification for Stainless Steel Bars and Shapes for Use in Boilers and Other Pressure Vessels
Classification Austenitic Stainless Steel
Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Mo N
Minimum Value - - - - - 16 10 2 0.1
Maximum Value 0.08 1 2 0.045 0.03 18 14 3 0.16
◎ New designations established in accordance with Practice E527 and SAE J1086 published jointly by ASTM and SAE. See ASTM DS-56C, available from ASTM Headquarters.
Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Reduction of Area
ψ
%
All specifications Annealing ≥550 ≥240 in 2 in.[50 mm] or 4D
≥ 30
≥ 40 ①
◎ d-diameter, t-thickness
1 Approximate Comparison Table Austenitic Stainless Steel
China Taiwan, China Japan South Korea United States Germany
GB ISC CNS JIS KS ASTM UNS DIN EN/DIN W-Nr.
06Cr17Ni12Mo2N
(0Cr17Ni12Mo2N)
S31658 316N SUS 316N STS 316N 316N S31651 X2CrNiMoN17-11-2 1.4406
2 Approximate Comparison Table Austenitic Stainless Steel
China Japan United States International Organization for Standardization European Standard
GB ISC JIS UNS ISO Numerical Grade Numerical Grade
06Cr17Ni12Mo2N S31658 SUS316N S31651 X6CrNiMoN17-12-3 4495-316-51-J (1.4495)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!