USA UNS S31700
ASTM
Specification or Grade
317
Corresponding Standard ASTM A479/A479M-2018
Standard Specification for Stainless Steel Bars and Shapes for Use in Boilers and Other Pressure Vessels
Classification Austenitic Stainless Steel
Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Mo
Minimum Value - - - - - 18 11 3
Maximum Value 0.08 1 2 0.045 0.03 20 15 4
◎ New designations established in accordance with Practice E527 and SAE J1086 published jointly by ASTM and SAE. See ASTM DS-56C, available from ASTM Headquarters.
Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Reduction of Area
ψ
%
All specifications Annealing ≥ 515 ① ≥205 in 2 in.[50 mm] or 4D
≥ 30
≥ 40 ②
◎ d-diameter, t-thickness
1 Approximate Comparison Table
China Taiwan, China Japan South Korea United States Germany United Kingdom
GB ISC CNS JIS KS ASTM UNS DIN EN/DIN W-Nr. BS EN/BS
06Cr19Ni13Mo3 S31708 317 SUS 317 STS 317 317 S31700 X5CrNiMo 17-13 1.4449 317S16
2 Approximate Comparison Table
China Taiwan, China Japan South Korea United States Germany United Kingdom
GB ISC CNS JIS KS ASTM UNS DIN EN/DIN W-Nr. BS EN/BS
06Cr19Ni13Mo3
(0Cr19Ni13Mo3)
S31708 317 SUS 317 STS 317 317 S31700 X5CrNiMo 17-13 1.4449 317S16
3 Approximate Comparison Table
China Japan United States International Organization for Standardization European Standard
ISC JIS UNS ISO Numerical Grade Numerical Grade
S31708 SUS317 S31700 X6CrNiMo19-13-4 4445-317-00-U (1.4445)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!