USA UNS S34565
Corresponding Standard ASTM A479/A479M-2018
Standard Specification for Stainless Steel Bars and Shapes for Use in Boilers and Other Pressure Vessels
Classification Austenitic Stainless Steel
Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Mo N Cb
Minimum Value - - 5 - - 23 16 4 0.4 -
Maximum Value 0.03 1 7 0.03 0.01 25 18 5 0.6 0.1
◎ New designations established in accordance with Practice E527 and SAE J1086 published jointly by ASTM and SAE. See ASTM DS-56C, available from ASTM Headquarters.
Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Reduction of Area
ψ
%
Hardness
HBW
All specifications Annealing ≥795 ≥415 in 2 in.[50 mm] or 4D
≥ 35
≥ 40 ① ≤230
◎ d-diameter, t-thickness
1 Approximate Comparison Table Austenitic Stainless Steel
China United States International Organization for Standardization European Standard
ISC UNS ISO Numerical Grade Numerical Grade
S34553 S34565 X2CrNiMnMoN25-18-6-5 4565-345-65-I 1.4565
2 Approximate Comparison Table Austenitic Stainless Steel
United States European Standard
UNS EN Numerical Grade
S34565 X2CrNiMnMoN25-18-6-5 1.4565

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!