USA UNS S82441
Corresponding Standard ASTM A479/A479M-2018
Standard Specification for Stainless Steel Bars and Shapes for Use in Boilers and Other Pressure Vessels
Classification Duplex Stainless Steel
Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu Mo N
Minimum Value - - 2.5 - - 23 3 0.1 1 0.2
Maximum Value 0.03 0.7 4 0.035 0.005 25 4.5 0.8 2 0.3
◎ New designations established in accordance with Practice E527 and SAE J1086 published jointly by ASTM and SAE. See ASTM DS-56C, available from ASTM Headquarters.
Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
d<11mm Annealing ≥740 ≥540 in 2 in.[50 mm] or 4D
≥ 25
≤290
d ≥ 11mm Annealing ≥680 ≥480 in 2 in.[50 mm] or 4D
≥ 25
≤290
◎ d-diameter, t-thickness
Approximate Comparison Table Austenitic-Ferritic Stainless Steel
United States International Organization for Standardization European Standard
UNS ISO Numerical Grade EN Numerical Grade
S82441 X2CrNiMnMoCuN24-4-3-2 4662-824-41-X X2CrNiMnMoCuN24-4-3-2 1.4662