USA UNS S44400
ASTM
Specification or Grade
444
Corresponding Standard ASTM A479/A479M-2018
Standard Specification for Stainless Steel Bars and Shapes for Use in Boilers and Other Pressure Vessels
Classification Ferritic Stainless Steel
Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Mo N More
Minimum Value - - - - - 17.5 - 1.75 - (Ti+Cb)
0.2+4×(C+N)~0.8
Maximum Value 0.025 1 1 0.04 0.03 19.5 1 2.5 0.035
◎ New designations established in accordance with Practice E527 and SAE J1086 published jointly by ASTM and SAE. See ASTM DS-56C, available from ASTM Headquarters.
Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Reduction of Area
ψ
%
Hardness
HBW
All specifications Annealing ≥415 ≥310 in 2 in.[50 mm] or 4D
≥ 20 ①
≥ 45 ①② ≤217
◎ d-diameter, t-thickness
Approximate Comparison Table
China Japan United States International Organization for Standardization France European Standard Sweden
ISC JIS ASTM UNS ISO Numerical Grade NF EN/NF EN Numerical Grade SS
S11972 SUS 444 444 S44400 X2CrMoTi18-2 4521-444-00-I Z3CDT18-02 X2CrMoTi18-2 1.4521 2326