USA UNS S44627
ASTM
Specification or Grade
XM-27
Corresponding Standard ASTM A479/A479M-2018
Standard Specification for Stainless Steel Bars and Shapes for Use in Boilers and Other Pressure Vessels
Classification Ferritic Stainless Steel
Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu Mo N Cb More
Minimum Value - - - - - 25 - - 0.75 - 0.05 (Ni+Cu)≤0.5
Maximum Value 0.01 0.4 0.4 0.02 0.02 27.5 0.5 0.2 1.5 0.015 0.2
◎ New designations established in accordance with Practice E527 and SAE J1086 published jointly by ASTM and SAE. See ASTM DS-56C, available from ASTM Headquarters.
Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Reduction of Area
ψ
%
Hardness
HBW
All specifications Annealing ≥450 ≥275 ≥ 45 ①② ≤217
◎ d-diameter, t-thickness
Approximate Comparison Table Ferritic Stainless Steel
China Japan United States International Organization for Standardization European Standard
ISC JIS UNS ISO Numerical Grade Numerical Grade
S12791 SUSXM27 S44627 X1CrMo26-1 4131-446-92-C (1.4131)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!