USA UNS S44700
Corresponding Standard ASTM A479/A479M-2018
Standard Specification for Stainless Steel Bars and Shapes for Use in Boilers and Other Pressure Vessels
Classification Ferritic Stainless Steel
Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu Mo N More
Minimum Value - - - - - 28 - - 3.5 - (C+N)≤0.025
Maximum Value 0.01 0.2 0.3 0.025 0.02 30 0.15 0.15 4.2 0.02
◎ New designations established in accordance with Practice E527 and SAE J1086 published jointly by ASTM and SAE. See ASTM DS-56C, available from ASTM Headquarters.
Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Reduction of Area
ψ
%
All specifications Annealing ≥485 ≥380 in 2 in.[50 mm] or 4D
≥ 20
≥ 40 ①
◎ d-diameter, t-thickness
Approximate Comparison Table Ferritic Stainless Steel
China Japan United States International Organization for Standardization European Standard
ISC JIS UNS ISO Numerical Grade Numerical Grade
S13091 SUS447J1 S44700 X1CrMo30-2 4135-447-92-C (1.4135)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!