◎ C-Cold rolled strip;H-Hot rolled strip;P-Hot rolled plate;T-Thickness;t-transverse;l-Longitudinal
◎ +A=annealed;+AT=solution annealed;+QT = quenched and tempered;+RA=recrystallizing annealed condition
◎ Austenitic steels always have adequate toughness and do not need to be impact tested. In contrast, austenitic-ferritic steels need to be tested to the impact energy requirements ensure that toughness is adequate.
* Resistance to intergranular corrosion when tested according to EN ISO 3651-2. In the delivery condition: yes;In the sensitized condition: yes.
① For continuously hot-rolled products, 20N/mm² higher minimum values of Rp0,2 and 10N/mm² higher minimum values of Rp1,0 may be agreed at the time of enquiry and order.
② If, in the case of strip in rolling widths < 300 mm, longitudinal test pieces are taken, the minimum values are reduced as download:proof strength: minus 15 N/mm²,elongation for constant gauge length: minus 5 %,elongation for proportional gauge length: minus 2 %
③ T<3mm:This value applies to specimens with a gauge length of 80 mm and a width of 20 mm. Specimens with a gauge length of 50 mm and a width of 12.5 mm may also be used. T ≥3mm:This value applies to specimens with a gauge length of 5.65√S