Grade En1A
Corresponding Standard BS 970-1955
Wrought steels in the form of bars, billets and forgings up to 6 in. ruling section for automobile and general engineering purpose
Classification Carbon Steel
En1A Chemical Element Composition Content (%)
Component C Si Mn P S
Minimum Value 0.07 - 0.8 - 0.2
Maximum Value 0.15 0.1 1.2 0.07 0.3
En1A Mechanical Properties
diameter or width across flats
d
mm
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Elongation or Extension Rate
δ
%
Bars; d≤13.5 Cold drawn or cold rolled ≥494 ≥10
Bars; 13.5<d≤38.1 Cold drawn or cold rolled ≥432 ≥14
Bars; 38.1<d≤63.5 Cold drawn or cold rolled ≥386 ≥14
Bar; 63.5<d≤101.6 Cold drawn or cold rolled ≥355 ≥14
Bar; d≤101.6 Rolling, normalizing or bright treatment ≥349 ≥26
• d-diameter or width across flats/mm
• The unit conversion for strength is based on: 1tons/sq.in=15.44N/mm2
• The unit conversion for impact energy absorption is based on: 1ft.lb=1.3558J

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!