Grade St70-2
Germany W-Nr. 1.0070
Old Grade
Corresponding Standard DIN 17100-1980
Steels for General Structural Purposes Quality Standard
Classification Carbon Steel
St70-2 Chemical Element Composition Content (%)
Component P S N
Minimum Value - - -
Maximum Value 0.05 0.05 0.009
①For product thickness t >100mm,C content according to the agreement
②For every 0.005% decrease in P below the specified maximum value, N may be increased by 0.001%. The nitrogen (N) content shall not exceed 0.012% in the ladle analysis and 0.014% in the product analysis.
③The content may not exceed 0.55%Si and 1 .60% Mn in the ladle analysis or 0.60%Si and 1 .70% Mn in the sample analysis.
St70-2 Mechanical Properties
thickness
t
mm
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
t<3 690~900 ≥365 3~8
3≤t≤16 670~830 ≥355 10~11
16<t≤40 670~830 ≥355 10~11
40<t≤63 670~830 ≥345 9~10
63<t≤80 670~830 ≥335 8~9
80<t≤100 670~830 ≥325 8~9
① Tensile test values apply to longitudinal specimens for steel with a width < 600 mm; for steel with a width ≥ 600 mm, transverse specimens shall be used.
② U=hot-rolled, non-heat-treated; N=normalized.
③ Impact energy absorption: The average of three tests is taken as the test result. The minimum average value is 23 or 27 J, and only one individual value is allowed to be up to 30% below the maximum (average) value.
New and Old Grade Replacement List
Corresponding Standard Grade
DIN 17100-1980
Grade
Germany W-Nr.
Old Grade
DIN EN 10025-2-2019
Grade
Germany W-Nr.
Approximate Comparison Table Carbon Structural Steel and Engineering Steel
China International Organization for Standardization Germany France European Standard Russia Sweden United Kingdom
GB ISO DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade GOST SS BS EN/BS
Q390C Fe690
FeE690
St70-2 1.0070 A70
A70-2
E360
Fe690-2①
1.0070 S375 1655-00
1655-01
E360
St70-2 Corresponding Standards(Same grade name, different standards)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!