Grade C85S
European Standard Steel Grade 1.1269
Corresponding Standard EN 10132-2021
Cold Rolled Narrow Steel Strip for Heat Treatment - Technical Delivery Conditions
Classification Spring Steel
C85S Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu Mo More
Minimum Value 0.8 0.15 0.4 - - - - - - Cr+Mo+Ni≤0.63
Maximum Value 0.9 0.35 0.7 0.025 0.025 0.4 0.4 0.3 0.1
① Elements not quoted in this table shall not be intentionally added to the steel without the agreement of the purchaser, other than for the purpose of finishing the heat. All reasonable precautions shall be taken to prevent the addition, from scrap or other material used in manufacture, of such elements which affect the hardenability, mechanical properties and application.
C85S Mechanical Properties
Delivery condition* Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
annealed (+A) or annealed and skin passed(+LC) ≤670 ≤535 ≥15 HV
≤210
cold rolled(+CR)** ≤1190 HV
≤325
quenched and tempered(QT)*** 1200~2000 HV
370~600
• The elongation values in the table are for a gauge length of 80 mm.
• +A=annealed,+LC=annealed and skin passed,+CR=cold rolled,+QT=quenched and tempered
Approximate Comparison Table Spring Steel
China Taiwan, China Japan South Korea United States International Organization for Standardization Germany France European Standard Russia Sweden United Kingdom
GB ISC CNS JIS KS AISI UNS ISO DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade GOST SS14 BS EN/BS
85 U20852 SUP3 SUP3 SPS1 1086 G10860 Type DC Ck85
C85S
1.1269
1.1269
XC85 C85S 1.1269 85A ≈1774 060A86
CS80
C85S Corresponding Standards(Same grade name, different standards)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!