Grade 350L0
Corresponding Standard AS /NZS 3679-1-1996
Part 1: Hot-Rolled Bars and Sections
Classification Carbon Steel
350L0 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu Mo Ti V Nb Al More
Minimum Value - - - - - - - - - - - - - Cu+Ni+Cr+Mo≤1;Nb+V≤0.03
Maximum Value 0.22 0.5 1.6 0.04 0.04 0.3 0.5 0.5 0.1 0.04 0.03 0.02 0.15
350L0 Mechanical Properties
thickness
t
mm
Heat Treatment or Condition
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Impact Energy Absorption
KV2
J
Flat steel, section steel; t<11 ≥480 ≥360 ≥20①
Flat steel, section steel; 11≤t<17 ≥480 ≥340 ≥20①
Flat steel, section steel; 17≤t<40 ≥480 ≥340 ≥20①
Flat steel, section steel; t≥40 ≥480 ≥330 ≥20①
Hexagonal steel, round steel, square steel; t≤50 ≥480 ≥340 ≥20①
Hexagonal steel, round steel, square steel; 50 < t ≤ 100 ≥480 ≥330 ≥20①
Hexagonal steel, round steel, square steel; t≥100 ≥480 ≥320 ≥20①
Sample dimensions 10mm×10mm 0°C
3 times average: ≥27
Single: ≥20
Sample dimensions 10mm×7.5mm 0°C
3 times average: ≥22
Single: ≥16
Sample dimensions 10mm×5mm 0°C
3 times average: ≥18
Single: ≥13
350L0 Corresponding Standards(Same grade name, different standards)