Grade GP240GH
European Standard Steel Grade 1.0619
Corresponding Standard EN 10213-2007(+A1:2016)
Steel Castings for Pressure Purposes
Classification Cast Steel
GP240GH Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu Mo V
Minimum Value 0.18 - 0.5 - - - - - - -
Maximum Value 0.23 0.6 1.2 0.03 0.02 0.3 0.4 0.3 0.12 0.03
GP240GH Mechanical Properties
thickness
t
mm
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Impact Energy Absorption
KV2
J
t ≤ 100 Normalizing (N)① 420~600 ≥240 A: ≥22 ≥27
t ≤ 100 Quenching + tempering (QT)② 420 ≥240 A: ≥22 ≥40
Approximate Comparison Table Cast Steel
China Germany European Standard
GB DIN EN/DIN EN Numerical Grade
ZG230-450 GS-C25N GP240GH 1.0619