Grade G24Mn6
European Standard Steel Grade 1.1118
Corresponding Standard EN 10213-2007(+A1:2016)
Steel Castings for Pressure Purposes
Classification Cast Steel
G24Mn6 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu Mo V
Minimum Value 0.2 - 1.5 - - - - - - -
Maximum Value 0.25 0.6 1.8 0.02 0.015 0.3 0.4 0.3 0.15 0.05
G24Mn6 Mechanical Properties
thickness
t
mm
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Impact Energy Absorption
KV2
J
t ≤ 100 Quenching + Tempering (QT2)① 650~800 ≥500 A: ≥15 Room temperature: ≥50
-30°C: ≥27
t ≤ 150 Quenching + Tempering (QT3)② 600~800 ≥400 A: ≥18 Room temperature: ≥60
-30°C: ≥27
G24Mn6 Corresponding Standards(Same grade name, different standards)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!