Grade G17CrMo9-10
European Standard Steel Grade 1.7379
Corresponding Standard EN 10213-2007(+A1:2016)
Steel castings for pressure purposes
Classification Cast Steel
G17CrMo9-10 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu Mo V
Minimum Value 0.13 - 0.5 - - 2 - - 0.9 -
Maximum Value 0.2 0.6 0.9 0.02 0.02 2.5 0.4 0.3 1.2 0.05
G17CrMo9-10 Mechanical Properties
thickness
t
mm
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Impact Energy Absorption
KV2
J
t ≤ 150 Quenching and Tempering (QT)① 590~740 ≥400 A: ≥18 ≥40
Approximate Comparison Table Heat-resistant cast steels and alloys
China United States United Kingdom
GB ASTM BS EN/BS
ZG17Cr2Mo1
GB/T 32255-2015
WC9
ASTM A217-2012
G17CrMo9-10
BS EN10213-2007
G17CrMo9-10 Corresponding Standards(Same grade name, different standards)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!