Grade GX2CrNi19-11
European Standard Steel Grade 1.4309
Corresponding Standard EN 10213-2007(+A1:2016)
Steel Castings for Pressure Purposes
Classification Cast Steel
GX2CrNi19-11 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu N
Minimum Value - - - - - 18 9 - -
Maximum Value 0.03 1.5 2 0.035 0.025 20 12 0.5 0.2
GX2CrNi19-11 Mechanical Properties
thickness
t
mm
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Impact Energy Absorption
KV2
J
t ≤ 150 Solution Heat Treatment + Water Quenching (AT)① 440~640 Rp1.0:≥210 A: ≥30 Room temperature: ≥80
-196°C: ≥70
Approximate Comparison Table Corrosion-Resistant Cast Steels
China Taiwan, China Japan South Korea United States International Organization for Standardization Germany France Russia United Kingdom
GB ISC CNS JIS KS ASTM UNS ISO DIN EN/DIN W-Nr. NF EN/NF GOST BS EN/BS
ZG03Cr18Ni10 C53043 SCS 19A SCS 36 SSC 19A CF3 J92500 GX2CrNi18-10 GX2CrNi19-11 1.4309 Z2CN18.10M 03Х18Н9Л 304C12
GX2CrNi19-11 Corresponding Standards(Same grade name, different standards)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!