Grade SUS302HQ
Classification Austenitic Stainless Steel
SUS302HQ Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni
Minimum Value - - - - - 17 8
Maximum Value 0.08 1 0.2 0.04 0.03 19 10
Approximate Comparison Table Stainless Steels for Cold Heading and Cold Extruding
China Japan South Korea United States International Organization for Standardization Germany
GB JIS KS ASTM/AISI ISO DIN EN/DIN
0Cr18Ni9Cu3 SUS302HQ STSXM7 XM7 X3CrNi18-9-4 X3CrNiCu18-9

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!