Grade 226M44
Corresponding Standard BS 970-3-1991
Specification for wrought steel for machanical and allied engineering purposes part 3:bright bars for general engineering purposes
Classification Carbon Steel
Properties Good Machinability
226M44 Chemical Element Composition Content (%)
Component C Si Mn P S
Minimum Value 0.4 - 1.3 - 0.22
Maximum Value 0.48 0.25 1.7 0.06 0.3
• For older grades of stainless steel, see Table 2 of standard BS 970-4-1970
226M44 Mechanical Properties
condition Mark
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
Impact Energy Absorption
KV2
J
6≤d<100 226M44R Quenching and Tempering + Turning or Grinding 700~850 ≥450 ≥16 201~255 Izod:≥27
KCV:≥22
6<d≤29 226M44T Quenching and Tempering + Turning or Grinding 775~925 ≥525 ≥14 223~277 Izod:≥20
KCV:≥16
6<d≤13 226M44S Quenching and Tempering + Turning or Grinding ④ 850~1000 ≥600 ≥12 248~302 Izod:≥20
KCV:≥16
6≤d<100 226M44R Quenching + Tempering + Cold Drawing or Quenching + Tempering + Cold Drawing + Grinding 700~850 ≥525 ≥12 201~255 Izod:≥27
6<d≤29 226M44T Quenching + Tempering + Cold Drawing or Quenching + Tempering + Cold Drawing + Grinding 775~925 ≥575 ≥10 223~277 Izod:≥20
6<d≤13 226M44S Quenching and tempering + cold drawing or quenching and tempering + cold drawing + grinding② 850~1000 ≥630 ≥9 248~302 Izod:≥20
226M44 Corresponding Standards(Same grade name, different standards)