Grade 430S17
Corresponding Standard BS 970-3-1991
Specification for wrought steel for machanical and allied engineering purposes part 3:bright bars for general engineering purposes
Classification Ferritic Stainless Steel
430S17 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu * Mo *
Minimum Value - - - - - 16 - - -
Maximum Value 0.08 1 1 0.04 0.03 18 0.5 0.3 0.3
• For older grades of stainless steel, see Table 2 of standard BS 970-4-1970
430S17 Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
Impact Energy Absorption
KV2
J
d≤63 750~820°C Annealing, Air Cooling ≥430 ≥280 ≥20 ≤170 -
Approximate Comparison Table Ferritic Stainless Steel
China Japan United States Germany France European Standard Russia Sweden United Kingdom
GB JIS ASTM UNS DIN EN/DIN NF EN/NF EN Numerical Grade GOST SS BS EN/BS
1Cr15 SUS430 430 S43000 X6Cr17 Z8C17 X6Cr17 1.4016 12KH17 2320 430S17