Grade X3CrNiCu18-9-4
European Standard Steel Grade 1.4567
Corresponding Standard EN 10263-5-2017
Steel rod, bars and wire for cold heading and cold extrusion - Part 5: Technical delivery conditions for stainless steels
Classification Austenitic Stainless Steel
Properties Corrosion Resistance
X3CrNiCu18-9-4 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu N
Minimum Value - - - - - 17 8.5 3 -
Maximum Value 0.04 1 2 0.045 0.03 19 10.5 4 0.1
X3CrNiCu18-9-4 Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Reduction of Area
ψ
%
Rod, Wire; 2<d≤5 Solid Solution + Cold Drawing + Solid Solution (+AT+C+AT) ≤600 ≥68
Wire; 2<d≤5 Solid Solution + Cold Drawn + Solid Solution + Quenched Rolling (+AT+C+AT+LC) ≤650 ≥63
Bar, rod, wire; 5<d≤10 Solid Solution (+AT) or Solid Solution + Decap (+AT+PE) ≤590 ≥68
Rod, wire; 5<d≤10 Solid Solution + Cold Drawn (+AT+C) ≤740 -
Rod, Wire; 5<d≤10 Solid Solution + Cold Drawing + Solid Solution (+AT+C+AT) ≤590 ≥68
Wire; 5<d≤10 Solid Solution + Cold Drawn + Solid Solution + Quenched Rolling (+AT+C+AT+LC) ≤640 ≥63
Bar, rod, wire; 10<d≤25 Solid Solution (+AT) or Solid Solution + Decap (+AT+PE) ≤590 ≥68
Rod, wire; 10<d≤25 Solid Solution + Cold Drawn (+AT+C) ≤700 -
Rod, Wire; 10<d≤25 Solid Solution + Cold Drawing + Solid Solution (+AT+C+AT) ≤590 ≥68
Bar, rod, wire; 25<d≤50 Solid Solution (+AT) or Solid Solution + Decap (+AT+PE) ≤590 ≥68
1 Approximate Comparison Table
China Taiwan, China Japan South Korea United States International Organization for Standardization Germany France European Standard
GB ISC CNS JIS KS ASTM/AISI UNS ISO Numerical Grade DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade
06Cr18Ni9Cu3 S30488 XM7 SUS XM7 STS XM7 XM7 S30430 X3CrNiCu 18-9-4 4567-304-30-I X3CrNiCu 18-9 1.4567 Z3CNU 18-10 X3CrNiCu 18-9-4 1.4567
2 Approximate Comparison Table
China Japan International Organization for Standardization European Standard
ISC JIS ISO Numerical Grade Numerical Grade
S30480 SUS304J1 X6CrNiCu17-8-2 4567-304-76-I 1.4567
3 Approximate Comparison Table
China Japan International Organization for Standardization European Standard
ISC JIS ISO Numerical Grade Numerical Grade
S30480 SUS304J3 X6CrNiCu18-9-2 4567-304-98-X 1.4567
4 Approximate Comparison Table
Japan United States France European Standard United Kingdom
JIS UNS NF EN/NF EN Numerical Grade BS EN/BS
SUSXM7 S30430 Z3CNU18-09FF
Z3CNU18-10
Z3CNU18-10FF
X3CrNiCu18-9-4 1.4567 304S17
5 Approximate Comparison Table Stainless steels for cold heading and cold extruding
China Japan International Organization for Standardization European Standard
GB ISC JIS ISO Numerical Grade EN Numerical Grade
06Cr18Ni9Cu2
(0Cr18Ni9Cu2)
S30480 SUS304J3 X6CrNiCu18-9-2 4567-304-98-X X6CrNiCu18-9-2 1.4567
6 Approximate Comparison Table Stainless steels for cold heading and cold extruding
China Japan International Organization for Standardization European Standard
GB ISC JIS ISO Numerical Grade EN Numerical Grade
06Cr18Ni9Cu3
(0Cr18Ni9Cu3)
S30488 SUSXM7 X3CrNiCu18-9-4 4567-304-30-I X3CrNiCu18-9-4 1.4567

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!