Grade 019Cr25Mo4Ni4NbTi
China ISC S12573
Corresponding Standard GB /T 32569-2016
Welded stainless steel tubes for seawater desalination plants
Classification Ferritic Stainless Steel
019Cr25Mo4Ni4NbTi Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Mo N More
Minimum Value - - - - - 24.5 3.5 3.5 - Ti+Nb:0.2+4(C+N)~0.8
Maximum Value 0.025 0.75 1 0.03 0.03 26 4.5 4.5 0.035
019Cr25Mo4Ni4NbTi Mechanical Properties
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
≥1000°C, rapid cooling ≥620 ≥515 ≥20 HRB: ≥100
019Cr25Mo4Ni4NbTi Corresponding Standards(Same grade name, different standards)