Grade GH2132
Corresponding Standard GB /T 40313-2021
Specification for Wrought Superalloy Forging Disks
Classification Special Alloy Steel
GH2132 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu Mo Ti V B Al More
Minimum Value - - 1 - - 13.5 24 - 1 1.8 0.1 0.001 - Fe:Remainder
Maximum Value 0.08 1 2 0.03 0.008 16 27 0.25 1.5 2.35 0.5 0.01 0.4
GH2132 Mechanical Properties
form Test Temperature Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Reduction of Area
ψ
%
Hardness
HBW
Impact Energy Absorption
KV2
J
sample Room Temperature ≥930 ≥615 ≥20 ≥30 255~321 KU2
≥23
sample High temperature long-term performance:
Stress 392MPa,
Creep fracture time ≥ 100h
1 Approximate Comparison Table Deformed High-Temperature Alloy
China United States Germany France Russia United Kingdom
GB ISC Commercial Grade AISI SAE AMS DIN EN/DIN W-Nr. L-Nr. NF EN/NF GOST BS EN/BS
GH2132
(GH132)
H21320 A286 AISI660 HEV7 5525
5731
5732
5734
5737
5895
X5NiCrTi 26-15 1.4980 1.4944 Z6NCT265
ATV SMo
ЭИ 786 DTD 5026
(S/ABV)
2 Approximate Comparison Table Deformed High-Temperature Alloy
China Japan United States Germany European Standard United Kingdom
GB JIS Commercial Grade UNS DIN EN/DIN W-Nr. EN Numerical Grade BS EN/BS
GH2132 SUH660 A286 S66286 X6NiCrTiMoVB25-15-2 1.4980 X6NiCrTiMoVB25-15-2 1.4980 X6NiCrTiMoVB25-15-2

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!