Grade GH4141
Corresponding Standard GB /T 40313-2021
Specification for Wrought Superalloy Forging Disks
Classification Special Alloy Steel
GH4141 Chemical Element Composition Content (%)
Component Fe C Si Mn P S Cr Mo Ti B Co Al Mg La More
Minimum Value - - - - - - 18 9 3 0.003 10 1.4 - - Ni:余量
Maximum Value 5 0.12 0.5 0.1 0.015 0.008 20 10.5 3.4 0.01 12 1.8 0.015 0.015
GH4141 Mechanical Properties
form Test Temperature Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Reduction of Area
ψ
%
Hardness
HBW
Impact Energy Absorption
KV2
J
sample Room Temperature (Disk Part) ≥1170 ≥880 ≥12 ≥12 ≥340 KU2
≥16
sample Room Temperature (Shaft Part) - - - - - KU2
≥16
sample 850°C (Disk Part) ≥740 ≥640 ≥12 ≥12 - -
sample 850°C (Disk Part) High-temperature endurance performance:
Stress 530MPa,
Creep rupture time tu≥0.5h
Creep Elongation After Fracture Au≥Measured
Approximate Comparison Table Deformed High-Temperature Alloy
China United States Germany France
GB ISC Commercial Grade AMS DIN EN/DIN W-Nr. NF EN/NF
GH4141
(GH141)
H41410 Rene 41 5545
5712
5513
5800
NiCr19CoMo 2.4973
2.4982
ATG W2
NC20KDTA
GH4141 Corresponding Standards(Same grade name, different standards)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!