Grade GH4738
Corresponding Standard GB /T 40313-2021
Specification for Wrought Superalloy Forging Disks
Classification Nickel and Nickel Alloys
GH4738 Chemical Element Composition Content (%)
Component Fe C Si Mn P S Cr Cu Mo N Ti Zr B Co Pb Al Sn Se Mg Bi Sb Ag Ca O Te More
Minimum Value - 0.02 - - - - 18 - 3.5 - 2.8 0.02 0.003 12 - 1.2 - - - - - - - - - Ni:余量;Tl≥0.0001;Al+Ti≥4.3
Maximum Value 2 0.05 0.15 0.1 0.015 0.002 21 0.1 5 0.005 3.3 0.08 0.01 15 0.001 1.6 0.005 0.0003 0.005 0.0001 0.0003 0.0005 0.005 0.002 5.0E-5
GH4738 Mechanical Properties
form Test Temperature Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Reduction of Area
ψ
%
Hardness
HBW
Impact Energy Absorption
KV2
J
sample Room Temperature ≥1250 ≥880 ≥15 ≥18 341~401 -
sample ≥1150 ≥830 ≥12 ≥18 - -
sample High temperature long-term performance:
Stress 550MPa,
Creep fracture time tu ≥ 23h
Notched sample creep fracture time tue > tu
Creep elongation after fracture Au ≥5
sample High temperature creep performance:
Stress 555MPa,
Creep elongation time tfx: 23h
Creep elongation Af ≤0.2
Approximate Comparison Table Deformed High-Temperature Alloy
China United States Germany France United Kingdom
GB ISC Commercial Grade UNS AMS DIN EN/DIN W-Nr. NF EN/NF BS EN/BS
GH4738
(GH738)
H47380 Waspaloy N07001 5704
5544
NiCr19Co14Mo4Ti 2.4654 ATG W1
NC20K14
NPK 50
GH4738 Corresponding Standards(Same grade name, different standards)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!