Grade 28Cr2Mo
GY4
Corresponding Standard GJB 1496B-2014
Classification Alloy Steel
28Cr2Mo Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu Mo
Minimum Value 0.25 0.18 0.3 - - 1.8 - - 0.25
Maximum Value 0.31 0.35 0.55 0.015 0.01 2.3 0.5 0.3 0.35
• Acid soluble boron content is 0.0003%~0.0005%.
28Cr2Mo Mechanical Properties
thickness
t
mm
Hardness
HBW
t=10~20 High Temperature Tempered or Hot Rolled Sample
HBW10/3000: ≤269
Indentation Diameter (mm): ≥3.7
t=25,30 High-temperature tempering or hot-rolled condition sample
HBW10/3000: ≤269
Indentation diameter mm: ≥3.7
Tempered sample
HBW10/3000: 341~285
Indentation diameter mm: 3.3~3.6

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!