Grade 314
USA UNS S31400
Corresponding Standard ASTM A959-2004
Standard Guide for Specifying Harmonized Standard Grade Compositions for Wrought Stainless Steels
Classification Austenitic Stainless Steel
Properties Corrosion Resistance Low-Temperature Toughness High-Temperature Strength Impact Toughness
314 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni
Minimum Value - 1.5 - - - 23 19
Maximum Value 0.25 3 2 0.045 0.03 26 22
Approximate Comparison Table Austenitic Heat-Resistant Steel
China United States International Organization for Standardization Germany France European Standard Russia United Kingdom
GB ISC UNS ISO DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade GOST BS EN/BS
16Cr25Ni20Si2
(1Cr25Ni20Si2)
S38340 S31400 X15CrNiSi 25-21 X15CrNiSi 25-20 1.4841 Z15CNS 25-20 X15CrNiSi 25-21 1.4841 20Х25Н20С2 310S24

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!