Grade 20Cr
Corresponding Standard GJB 1220A-2008
Speification for alloy structure steel bar for artillery parts
Classification Alloy Steel
20Cr Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu
Minimum Value 0.18 0.17 0.5 - - 0.7 - -
Maximum Value 0.24 0.37 0.8 0.03 0.03 1 0.3 0.25
20Cr Mechanical Properties
diameter
d
mm
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Reduction of Area
ψ
%
Hardness
HBW
Impact Energy Absorption
KV2
J
d=15 880°C First Quenching, 780~820°C Second Quenching, Water or Oil Cooling, 200°C Tempering, Water or Air Cooling ≥835 ≥540 ≥10 ≥40 - KU2
≥47
Steel Annealing or Tempering - - - - ≤179 -

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!