Grade 20CrMnTi
Corresponding Standard GJB 1220A-2008
Speification for alloy structure steel bar for artillery parts
Classification Alloy Steel
20CrMnTi Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu Ti
Minimum Value 0.17 0.17 0.8 - - 1 - - 0.04
Maximum Value 0.23 0.37 1.1 0.03 0.03 1.3 0.3 0.25 0.1
20CrMnTi Mechanical Properties
diameter
d
mm
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Reduction of Area
ψ
%
Hardness
HBW
Impact Energy Absorption
KV2
J
d=15 880°C First Quenching, 870°C Second Quenching, Oil Cooling, 200°C Tempering, Water or Air Cooling ≥1080 ≥850 ≥10 ≥45 - KU2
≥55
Steel Annealing or Tempering - - - - ≤217 -

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!