Grade 37CrNi3A
Corresponding Standard GJB 1220A-2008
Speification for alloy structure steel bar for artillery parts
Classification Alloy Steel
37CrNi3A Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu
Minimum Value 0.34 0.17 0.25 - - 1.2 3 -
Maximum Value 0.41 0.37 0.55 0.025 0.025 1.6 3.5 0.25
37CrNi3A Mechanical Properties
diameter
d
mm
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Reduction of Area
ψ
%
Hardness
HBW
Impact Energy Absorption
KV2
J
d=25 820°C quenching, oil cooling, 500°C tempering, water or oil cooling ≥1130 ≥980 ≥10 ≥50 - KU2
≥47
Steel Annealing or Tempering - - - - ≤269 -