Grade 40CrMnMo
Corresponding Standard GJB 1220A-2008
Speification for alloy structure steel bar for artillery parts
Classification Alloy Steel
40CrMnMo Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu Mo
Minimum Value 0.37 0.17 0.9 - - 0.9 - - 0.2
Maximum Value 0.45 0.37 1.2 0.03 0.03 1.2 0.3 0.25 0.3
40CrMnMo Mechanical Properties
diameter
d
mm
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Reduction of Area
ψ
%
Hardness
HBW
Impact Energy Absorption
KV2
J
d=15 850°C Quenching, Oil Quenching, 600°C Tempering, Water or Oil Quenching ≥980 ≥785 ≥10 ≥45 - KU2
≥71
Steel Annealing or Tempering - - - - ≤217 -