A681 Type H19 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Mo W V Co More
Minimum Value 0.32 0.15 0.2 - - 4 0.3 3.75 1.75 4 Ni+Cu≤0.75
Maximum Value 0.45 0.5 0.5 0.03 0.03 4.75 0.55 4.5 2.2 4.5
A681 Type H19 Mechanical Properties
form Heat Treatment or Condition
Hardness
HBW
Bars, thick plates, thin plates, strips, rods, wires, forgings Cold Drawing BHN
≤262
Bars, thick plates, thin plates, strips, rods, wires, forgings Annealing BHN
≤241
Bars, thick plates, thin plates, strips, rods, wires, forgings Heat Treatment HRC
≥55