Grade 08Cr4Mo
China ISC A30081
Corresponding Standard GB /T 37618-2019
Nitriding Steels
Classification Alloy Steel
08Cr4Mo Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu Mo
Minimum Value 0.04 0.17 0.85 - - 3.7 - - 0.4
Maximum Value 0.12 0.37 1.2 0.03 0.03 4.3 0.3 0.3 0.6
08Cr4Mo Mechanical Properties
test size
d
mm
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
Impact Energy Absorption
KV2
J
d=25 Quenching temperature 940~960°C, water cooling; tempering temperature 620~660°C, water or oil cooling ≥800 ≥700 ≥14 Normalizing + Tempering, Annealing or High Temperature Tempering Condition Delivered Steel Rod
≤220
≥35

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!