Grade 40Cr3MoV
China ISC A31401
Corresponding Standard GB /T 37618-2019
Nitriding Steels
Classification Alloy Steel
40Cr3MoV Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu Mo V
Minimum Value 0.36 0.17 0.4 - - 3 - - 0.8 0.15
Maximum Value 0.43 0.37 0.7 0.03 0.03 3.5 0.3 0.3 1.1 0.25
40Cr3MoV Mechanical Properties
test size
d
mm
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
Impact Energy Absorption
KV2
J
d=25 Quenching temperature 870~970°C, oil or water quenching; tempering temperature 580~700°C, water or oil quenching ≥950 ≥750 ≥11 Normalizing + Tempering, Annealing or High Temperature Tempering Condition Delivered Steel Rod
≤248
≥25

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!