Grade 34Cr2Ni1MoAl
China ISC A57341
Corresponding Standard GB /T 37618-2019
Nitriding steels
Classification Alloy Steel
34Cr2Ni1MoAl Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu Mo Al
Minimum Value 0.3 0.17 0.4 - - 1.5 0.85 - 0.15 0.8
Maximum Value 0.37 0.37 0.7 0.03 0.03 1.8 1.15 0.3 0.25 1.2
34Cr2Ni1MoAl Mechanical Properties
test size
d
mm
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
Impact Energy Absorption
KV2
J
d=25 Quenching temperature 870~930°C, oil/water cooling; tempering temperature 580~700°C, water/oil cooling ≥900 ≥680 ≥10 Normalizing + Tempering, Annealing or High Temperature Tempering Condition Delivered Steel Rod
≤248
≥30