Grade SS317L
Corresponding Standard EN ISO 14343-2017
Welding Consumables — Wire Electrodes, Strip Electrodes, Wires and Rods for Arc Welding of Stainless and Heat Resisting Steels — Classification
Classification Austenitic Stainless Steel
SS317L Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu Mo
Minimum Value - 0.3 1 - - 18.5 13 - 3
Maximum Value 0.03 0.65 2.5 0.03 0.03 20.5 15 0.75 4
SS317L Mechanical Properties
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
≥480 ≥300 ≥25

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!