Grade SA-213 Grade TP304H
S30409
Corresponding Standard ASME SA-213/SA-213M-2019
Standard Specification for Seamless Ferritic and Austenitic Alloy-Steel Boiler,Superheater, and Heat-Exchanger Tubes
Classification Alloy Steel
SA-213 Grade TP304H Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni
Minimum Value 0.04 - - - - 18 8
Maximum Value 0.1 1 2 0.045 0.03 20 11
SA-213 Grade TP304H Mechanical Properties
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
≥515 ≥205 ≥35 HBW: ≤192
HV:: ≤200
HRB: ≤90
1 Approximate Comparison Table Austenitic Stainless Steel
China Japan United States International Organization for Standardization Germany European Standard
GB ISC JIS AISI UNS ISO DIN EN/DIN W-Nr. EN Numerical Grade
07Cr19Ni10 S30409 SUS 304H 304H S30409 X6CrNi 18-10
X7CrNi 18-9
X6CrNi18-10 1.4948 X6CrNi18-10 1.4948
2 Approximate Comparison Table
Japan United States International Organization for Standardization France European Standard Russia
JIS ASTM UNS ISO NF EN/NF EN Numerical Grade GOST
SUS304H 304H S30409 X7CrNi18-9 Z6CN18-09 X6CrNi18-10 1.4948 08KH18N10

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!