Grade G17Mn5
Germany W-Nr. 1.1131
Corresponding Standard DIN EN 10293-2005
Steel castings for general engineering uses
Classification Cast Steel
G17Mn5 Chemical Element Composition Content (%)
Component C Si Mn P S *
Minimum Value 0.15 - 1 - -
Maximum Value 0.2 0.6 1.6 0.02 0.02
G17Mn5 Mechanical Properties
thickness
t
mm
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Impact Energy Absorption
KV2
J
t≤50 Quenching + Tempering (+QT)
Quenching temperature 920~980°C air or liquid cooling, Tempering temperature 600~700°C
450~600 ≥240 ≥24 -30°C: ≥27
Room Temperature: ≥70
New and Old Grade Replacement List
Corresponding Standard Grade
DIN 17182-1992
Grade
Germany W-Nr.
DIN EN 10293-2005
Grade
Germany W-Nr.
G17Mn5 Corresponding Standards(Same grade name, different standards)