Grade EN-GJS-400-18-RT
European Standard Steel Grade 5.3104
Other Names
Corresponding Standard EN 1563-2018
Spheroidal Graphite Cast Irons
Classification cast Iron
Density 7.1 g/cm3
EN-GJS-400-18-RT Mechanical Properties
condition Mark
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Impact Energy Absorption
KV2
J
Casting specimen; t≤30 EN-GJS-400-18-RT ≥400 ≥250 ≥18 (23 ± 5) °C
Average of 3 samples: ≥14
Single sample value: ≥11
Casting specimen; 30<t≤60 EN-GJS-400-18-RT ≥390 ≥250 ≥15 (23 ± 5) °C
Average of 3 samples: ≥14
Single sample value: ≥11
Casting sample; t>60 EN-GJS-400-18-RT ≥370 ≥240 ≥12 (23 ± 5) °C
Average value of 3 samples: ≥ 12
Individual sample value: ≥ 9
Base specimen; t≤30 EN-GJS-400-18C-RT ≥390 ≥250 ≥15
Base specimen; 30<t≤60 EN-GJS-400-18C-RT ≥370 ≥240 ≥12
Body sample; 60<t≤200 EN-GJS-400-18C-RT ≥350 ≥230 ≥10
• Samples cut from the casting the letter “C” is added at the end of the designation by symbol. e.g. EN-GJS-800-2C
Approximate Comparison Table Cast Iron
International Organization for Standardization European Standard
ISO EN Numerical Grade
400-18
400-18-RT/S
400-18-RT/U
EN-GJS-400-18-RT 5.3104
(EN-JS1024)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!