Grade EN-GJS-500-7
European Standard Steel Grade 5.3200
Other Names
Corresponding Standard EN 1563-2018
Classification cast Iron
Density 7.1 g/cm3
EN-GJS-500-7 Mechanical Properties
condition Mark
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
Casting specimen; t≤30 EN-GJS-500-7 ≥500 ≥320 ≥7
Casting specimen; 30<t≤60 EN-GJS-500-7 ≥450 ≥300 ≥7
Casting samples; 60<t≤200 EN-GJS-500-7 ≥420 ≥290 ≥5
Base specimen; t≤30 EN-GJS-500-7C ≥480 ≥300 ≥6
Base specimen; 30<t≤60 EN-GJS-500-7C ≥450 ≥280 ≥5
Body sample; 60<t≤200 EN-GJS-500-7C ≥400 ≥260 ≥3
Castings; t≤60 170~230
Castings; 60 < t ≤ 200 150~230
• Samples cut from the casting the letter “C” is added at the end of the designation by symbol. e.g. EN-GJS-800-2C
Approximate Comparison Table cast iron
China Japan United States International Organization for Standardization Germany France European Standard Russia Sweden United Kingdom Australia
GB JIS ASTM ISO DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade GOST SS BS EN/BS Australian Standard AS
QT500-7 FCD500
FCD500-7
65-45-12
70-50-05
80-55-06
500-7
500-7/S
500-7/U
GGG50 0.7050 500-7
FGS500-7
EN-GJS-500-7 5.3200
(EN-JS1050)
VCH50 0727-02
27-02
500/7 500-7
EN-GJS-500-7 Corresponding Standards(Same grade name, different standards)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!