Grade EN-GJS-600-3
European Standard Steel Grade 5.3201
Other Names
Corresponding Standard EN 1563-2018
Spheroidal Graphite Cast Irons
Classification cast Iron
Density 7.1 g/cm3
EN-GJS-600-3 Mechanical Properties
condition Mark
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
Casting specimen; t≤30 EN-GJS-600-3 ≥600 ≥370 ≥3
Casting specimen; 30<t≤60 EN-GJS-600-3 ≥600 ≥360 ≥2
Casting samples; 60<t≤200 EN-GJS-600-3 ≥550 ≥340 ≥1
Base specimen; t≤30 EN-GJS-600-3C ≥580 ≥360 ≥3
Base specimen; 30<t≤60 EN-GJS-600-3C ≥550 ≥340 ≥2
Body sample; 60<t≤200 EN-GJS-600-3C ≥500 ≥320 ≥1
Castings; t≤60 190~270
Castings; 60 < t ≤ 200 180~270
• Samples cut from the casting the letter “C” is added at the end of the designation by symbol. e.g. EN-GJS-800-2C
Approximate Comparison Table Cast Iron
China Japan United States International Organization for Standardization Germany France European Standard Russia Sweden United Kingdom Australia
GB JIS ASTM ISO DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade GOST SS BS EN/BS Australian Standard AS
QT600-3 FCD600
FCD600-3
100-70-03
80-55-06
80-60-03
600-3
600-3/S
600-3/U
GGG60 0.7060 600-3
FGS600-3
EN-GJS-600-3 5.3201
(EN-JS1060)
VCH60 0732-03
32-03
600/3 600-3
EN-GJS-600-3 Corresponding Standards(Same grade name, different standards)