Grade 65
China ISC U20652
Other Names
Corresponding Standard GB /T 699-1999
Quality Carbon Structural Steels
Classification Carbon Steel
Properties Strength Hardness Elasticity
65 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu
Minimum Value 0.62 0.17 0.5 - - - - -
Maximum Value 0.7 0.37 0.8 0.035 0.035 0.25 0.3 0.25
① The grades listed in the table are of high quality steel. High quality steel, in the grade suffix A, the last digit of the unified digital code is changed to 3; Super high quality steel, in the grade suffix E, the last digit of the unified digital code is changed to 6; The rimming steel, grade suffix F, the last digit of the unified digital code is changed to 0; Semi-killed steel, grade suffix b, unified number code last digit is 1
qulity steel P≤0.035%,S≤0.035%
high qulity steel P≤0.035%,S≤0.035%
speicial high qulity steel P≤0.025%,S≤0.020%
② 08 steel with aluminum deoxidation smelting killed steel, the lower limit of manganese content is 0.25%, silicon content is not more than 0.03%, aluminum content is 0.02%~0.07%, this time the steel grade is 08Al
③ Upon agreement between supply and demand parties, 08~25 steel can be supplied as semi-killed steel with silicon content not exceeding 0.17%, with the grade designations of 08b~25b.
④ Steel produced from scrap metal may have a copper content of no more than 0.30%; the copper content in steel for hot-pressure processing should not exceed 0.20%.
⑤ The silicon content of the rimming steels which used for cold pressing shall be not more
than 0.03%.
⑥ Steel produced by oxygen converter process should have a nitrogen content of no more than 0.008%.
65 Mechanical Properties
diameter(thickness)
d
mm
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
d=25 (sample size) Normalizing
≥695
Normalizing
≥410
Normalizing
≥10
Unprocessed Steel
≥255
Annealed Steel
≤229
① For steel with a diameter or thickness of less than 25mm, heat treatment is performed on a sample blank with the same cross-section size as the finished product
② Table normalizing recommended holding time is not less than 30min, air cooling; The recommended holding time for quenching is not less than 30min,70, 80 and 85 steel oil cooling, and the other steel water cooling; The recommended holding time for tempering is not less than 1h.
1 Approximate Comparison Table High-Quality Carbon Structural Steel
China United States International Organization for Standardization Germany France Russia Sweden United Kingdom
GB ISC ASTM/AISI UNS ISO DIN EN/DIN W-Nr. NF EN/NF GOST SS BS EN/BS
65 U20652 1065 G10650 SL
SM
Ck67 1.1231 XC65 65 1770 060A67
2 Approximate Comparison Table Spring Steel
China Japan United States International Organization for Standardization Germany France Russia Sweden United Kingdom
GB ISC JIS AISI UNS ISO DIN EN/DIN W-Nr. NF EN/NF GOST SS14 BS EN/BS
65 U20652 SUP2 1065 G10650 Type DC Ck67 1.1231 XC65 65 1770 060A67
3 Approximate Comparison Table High-Quality Carbon Structural Steel
China United States France Russia United Kingdom
GB ASTM/AISI NF EN/NF GOST BS EN/BS
65
(GB/T 699-1999)
1064
1065
C65
XC65
65 060A67
4 Approximate Comparison Table Spring Steel
China Japan United States International Organization for Standardization European Standard
GB ISC JIS ASTM/AISI ISO EN Numerical Grade
65
(GB/T 1222-2016)
U20652 S65-CSP
(JIS G4802:2005)
1065
(ASTM A29/A29M:2005)
C60E4
(ISO 683-18:1996)
C60E
(EN 10083-1:1991+A1:1996)
1.1221
5 Approximate Comparison Table Spring Steel 1
China Germany France Russia United Kingdom
GB W-Nr. L-Nr. NF EN/NF GOST BS EN/BS
65 CK65 1.1235 XC65 65 080A67

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!