Grade FCD 350-22L
Corresponding Standard JIS G 5502-2022
Spheroidal Graphite Cast Irons
Classification cast Iron
FCD 350-22L Mechanical Properties
thickness
t
mm
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Impact Energy Absorption
KV2
J
Casting; t≤30; single cast and side by side or continuous cast specimen ≥350 ≥220 ≥22 -40°C ± 2°C
Average of 3 samples: ≥12
Single sample: ≥9
Castings; 3<t≤60; single casting and side-by-side or continuous casting samples ≥330 ≥210 ≥18 -40°C ± 2°C
Average of 3 samples: ≥12
Single sample: ≥9
Castings; 60<t≤200; single casting and side-by-side or continuous casting samples ≥320 ≥200 ≥15 -40°C±2°C
Three samples: ≥10
Individual sample: ≥7
casing; t ≤ 30; casting machining sample ≥340 ≥220 ≥20
casing; 30 < t ≤ 60; casting machining sample ≥320 ≥210 ≥15
casing; 60 < t ≤ 200; casting machining sample ≥310 ≥200 ≥12
Approximate Comparison Table Cast Iron
Japan International Organization for Standardization Germany France European Standard Sweden United Kingdom
JIS ISO DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade SS BS EN/BS
FCD350-22L 350-22
350-22-LT/S
350-22-LT/U
350-22L
GGG35.3 0.7033 350/22L40
FGS-370-17
EN-GJS-350-22-LT 5.3100
(EN-JS1015)
17-15 350/22L40
370/17

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!