Grade WPNIC11
USA UNS N08811
Corresponding Standard ASTM A403/A403M-2022
Wrought Austenitic Stainless Steel Piping Fittings
Classification Austenitic Stainless Steel
WPNIC11 Chemical Element Composition Content (%)
Component Fe C Si Mn P S Cr Ni Cu Ti Al More
Minimum Value 39.5 0.06 - - - - 19 30 - 0.25 0.25 Al+Ti: 0.85~1.2
Maximum Value - 0.1 1 1.5 0.04 0.015 23 35 0.75 0.6 0.6
WPNIC11 Mechanical Properties
condition Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Pipe Fittings ≥450 ≥170 Standard round specimen, or small specimen, or strip specimen
L0=4D
long: ≥28
tr: ≥20
1 Approximate Comparison Table Corrosion-Resistant Alloy
China United States
GB ISC Commercial Grade UNS
NS 1104 H 08811 Incoloy 800HT N 08811
2 Approximate Comparison Table Austenitic Stainless Steel
United States International Organization for Standardization European Standard
UNS ISO Numerical Grade Numerical Grade
N08811 X8NiCrAlTi33-21 4959-088-11-U 1.4959
3 Approximate Comparison Table Corrosion-Resistant Alloy
United States Germany
Commercial Grade UNS DIN EN/DIN W-Nr.
Incoloy 800HT N08811 X8NiCrAlTi32-21 1.4959

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!