Grade En15A
Corresponding Standard BS 970-1955
Wrought Steels IN THE FORM OF BARS, BILLETS AND FORGINGS UP TO 6 IN. RULING SECTION FOR AUTOMOBILE AND GENERAL ENGINEERING PURPOSE
Classification Carbon Steel
En15A Chemical Element Composition Content (%)
Component C Si Mn P S
Minimum Value 0.3 0.05 1.3 - -
Maximum Value 0.4 0.35 1.7 0.06 0.06
En15A Mechanical Properties
diameter or width across flats
d
mm
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
Impact Energy Absorption
KV2
J
Bar, billet, forged product; d ≤ 101.6 Quenching and Tempering Q ≥618 ≥432 ≥22 179~229 ≥34
Bars, Billets, Forgings; d≤63.5 Quenching and Tempering R ≥695 ≥525 ≥20 201~255 ≥34
Bars, billets, forgings; d≤22.2 Quenching and Tempering S ≥772 ≥587 ≥20 223~277 ≥34
• d-diameter or width across flats/mm
• The unit conversion for strength is based on: 1tons/sq.in=15.44N/mm2
• The unit conversion for impact energy absorption is based on: 1ft.lb=1.3558J

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!